“It’s been scientifically proven that the temp of the shingles rises only a couple of degrees when there is an unvented attic compared to a vented attic,” said Garry Barlow, estimator at RetroFoam of Michigan. “If we lived in a southern state it has been proven that the longevity of the shingle did diminish by only one year. In the northern states there was no difference in the life span of the shingles.”
Part of that guidance will be explaining that interior, two component foam is applied with the professional using specific personal protective equipment (high-pressure foam is installed while using a respirator, for example). It is encouraged that professionals explain clearly to customers that this equipment, coupled with certain work and engineering practices, including ventilation, is used to minimize exposures to the chemicals used to make SPF during the job.
SPF insulation applied by professionals is usually described as either a high- or low-pressure foam and is available as either open- or closed-cell. Each type has advantages and disadvantages depending on the application requirements. The comparison chart below can be helpful in explaining or understanding which type of SPF insulation is best suited to a specific application.

Allison--would be very interested in your take on the GHG issues of foams, which have received lots of smart commentary recently. To highlight a few: architect Jesse Thompson's comments on Tom's Good vs Bad post on Energy Circle, the very thorough piece by Alex Wilson on Green Building Advisor and Michael Anschel's cautionary diatribe on Remodeling. 


Roof coatings are easy to install. Smaller roofs in good, serviceable condition can be a weekend do-it-yourself (DIY) project. Larger roofs with leaks and ponding water issues should be coated by a qualified professional. Additional roof coating products, such as foam or coatings designed for seams, may be required underneath the main coating layers. Supplement coating products are used to reinforce damaged or leak-prone problem areas.[3]

Sta-Kool 780 Siliconized Acrylic White Elastomeric Roof Coating Sta-Kool 780 Siliconized Acrylic White Elastomeric Roof Coating is a high quality flexible white acrylic roof coating. Product is enhanced with silicone for improved water resistance adhesion and life expectancy. Product resists cracking peeling while offering tremendous durability and long term life. The coating forms a durable protective barrier which ...  More + Product Details Close https://www.youtube.com/watch?feature=youtube.be&v=ggLAUsiuI_o
This website uses cookies and other tracking technologies (also known as pixels or beacons) to aid your experience (such as viewing videos), as well as “performance cookies” to analyze your use of this website and to assist with marketing efforts. If you click the “Accept All Cookies” button or continue navigating the website, you agree to having those first and third-party cookies set on your device. If you do not wish to accept cookies from this website, you can choose to not allow cookies from this website by updating your browser preferences. For more information on how we use Cookies, please read our Privacy Policy.

The problem you saw with the closed cell foam pulling away like that is due to the heat of the foam was to hot. It was actually curing out and making foam before it could adhere to the wood. The installer wasn't reading his foam correctly. He should of stopped and turned down the heat on his hose temp. Also installers have to be aware that as the sun rises and the temp in attics rises the subtrates get hotter as well. This will cause the installer to adjust his heat when installing the foam as the temp changes thru out the day.  


We live in middle TN and had our house foamed last year. We noticed recently that some of the foam was shrinking and seperating from the floor joists. We contacted the installer and he informed us that the manufacturer had a problem with a batch of foam during the time frame we had our house sprayed. The contractor wasn't sure if we had the recalled batch installed in our house or not. He said he would check the batch numbers and let us know. He seems like a nice guy promising to do whatever it takes to fix any problems. Do we trust him, however, to be truthful about the batch number? Do we have any options for finding out the information ourselves? I inspected the entire crawl space of the house and noticed approximately (5) areas that were seperating and a couple areas where the foam didn't adhere to the block. Do I assume by it being so infrequent that it is nothing to be concerned about? My concern is the walls that are not capable of being visually inspected because of sheetrock. 

The problem was that the installer was doing his first spray foam job ever, and the thickness of the insulation varied from zero (visible roof deck) to about 9". Unfortunately, good average thickness doesn't cut it. The coverage needs to be uniform because a lot of heat will go through the under-insulated areas. (See my article on flat or lumpy insulation performance.)


It also has a great waterproofing ability that can shield the roof’s membrane from water and moisture damage. You can also count on the liquid roof coating for its outstanding performance for a wide range of applications and uses. This product can be used at tears and seams as well as in sealing air conditioners and venting systems and anywhere else where rubberized coating is needed.